結(jié)構(gòu)膠混合不均勻,局部會出現(xiàn)白色條紋。在光線比較亮的情況下,更加容易觀察。今天雙組份打膠機(jī)廠家的小編給大家講解一下膠體混合不均勻的原因,希望對大家有所幫助!
Structural adhesives are unevenly mixed and white stripes appear locally. It is easier to observe when the light is brighter. Today, the small edition of the two-component glue beater manufacturer explains the reason why the colloid mixing is not uniform. I hope it will be helpful to you all.
①連續(xù)花膠:一般是混合器堵塞、混合器裝配錯誤或者使用的混合單元不夠多;
(1) Continuous gum: generally, the mixer is blocked, the mixer assembly is wrong or the mixing unit is not enough;
②斷續(xù)有規(guī)律花膠:與系統(tǒng)性故障有關(guān),如配比泵密封泄漏或者比例架磨損;
(2) Intermittent regular pattern gum: related to systemic faults, such as leakage of seal of proportioning pump or wear of proportioning frame;
③斷續(xù)無規(guī)律花膠:與故障有關(guān),如過濾器堵塞/針閥堵塞/壓盤故障/配比泵入口堵塞或者密封失效/安全閥及高壓球閥失效等;
(3) Discontinuous irregular pattern gum: related to faults, such as filter blockage/needle valve blockage/platen failure/ratio pump entrance blockage or seal failure/safety valve and high pressure ball valve failure;

雙組份打膠機(jī)
④短暫停槍后又開槍時,開頭出現(xiàn)一段花膠:主要是膠粘度匹配不理想,需要調(diào)整系統(tǒng)管道或降低工作壓力。
(4) When the gun stops for a short time and fires again, a section of gum appears at the beginning: the main reason is that the gum viscosity matching is not ideal, and the system pipeline needs to be adjusted or the working pressure should be reduced.
打膠機(jī)要定期進(jìn)行保養(yǎng),確保打膠機(jī)可以正常工作。每次開機(jī)前必須做蝴蝶試驗,確保結(jié)構(gòu)膠混合均勻。蝴蝶試驗的方法如下:將打膠機(jī)打出的混合好的膠擠到紙中間5-10克,折合紙將膠壓平。打開紙檢查膠樣,混合均勻的膠應(yīng)無異色條紋,如果膠出現(xiàn)異色條紋,則表明混膠不均勻,應(yīng)查找原因,問題解決后才能使用。
The gluing machine should be regularly maintained to ensure that the gluing machine can work properly. Butterfly test must be done before starting each machine to ensure that the structural glue mixes evenly. The butterfly test method is as follows: the mixed glue produced by the gluer is squeezed into the middle of the paper for 5-10 grams, and the folding paper is pressed flat. Open the paper and check the rubber sample. The glue with uniform mixing should have no heterochromatic stripes. If there are heterochromatic stripes in the glue, it shows that the mixing is not uniform. The reason should be found out and the problem can be solved before using it.
本文的精彩內(nèi)容由雙組份打膠機(jī)的小編進(jìn)行整理編寫,本公司堅持以誠信合作的共贏理念,為您提供的服務(wù),歡迎點擊進(jìn)入:http://linshi.jncsjx.com
The wonderful content of this article is compiled by the small edition of the two-component glue machine. Our company adheres to the win-win concept of honesty and cooperation, and provides you with perfect service. Welcome to http://linshi.jncsjx.com.

聯(lián)系我們Contact us

  • 咨詢熱線:0531-85717458 13705446998
  • 公司地址: 山東省德州市齊河安頭鄉(xiāng)企巢工業(yè)園
  • 掃碼聯(lián)系我們:

截屏,微信識別二維碼

微信號:13705446998

//